Publish Time: 2026-07-02 Origin: Site
Uneven Veneer Thickness
Peeling due to uneven thickness of the veneer is one of the most common faults. It is usually caused when the knife adjustment is not set properly, hydraulic pressure remains uneven, worn pressure rollers or poor log centering. Frequent calibration with knife position helps keeping hydraulic pressure stable, and feeding system inspection ensures veneer thickness reaches standard.
Veneer Cracking and Splitting
This will create cracks and splits if they are too dry, not tenderized enough, or peeled at the wrong settings. Veneer cracking can be reduced significantly and overall quality improved by: Correct log conditioning, optimising the tenderising process, using a sharp peeling knife as well as correct adjustment of the peeling speed.
Rough Veneer Surface
Bumpy bark is typically a result of a dull knife, the incorrect angle of the knife relative to the log, spinning too quickly or the log rotating out of balance. With a sharp knife, correct cutting angle and smooth roller operation, they produce clean, smooth veneer with minimal surface defects.
Frequent Veneer Breakage
Some of the causes of veneer breakage include tension, wooden rollers being set too tightly and on low quality logs or machine settings not optimal. The efficient processing is based on designing methods that diminish peeling stresses, adjusting the roller pressure appropriately, and choosing adequate logs while keeping a machine stable to minimize veneer losses.
Higher Residual Core and Lower Veneer Recovery
How a large residual core results into extensive wood allowing high prices. This issue can be caused by poor machine calibration, worn rollers or peeling parameters that have not been adjusted correctly. Proper maintenance, accurate hydraulic settings and proper knife positioning enable it to peel closer to the center of the log, maximizing veneer recovery and increasing raw material efficiency.